Skip to content

Plast-O-Fix 90 black 50ml, 2 pieces

SKU 409516-2
Original price €52,81 - Original price €52,81
Original price Logge dich ein, um Preise zu sehen
Logge dich ein, um Preise zu sehen
€52,81 - Logge dich ein, um Preise zu sehen
Current price Logge dich ein, um Preise zu sehen
Plast-O-Fix 90 black 50ml, 2 KTU

Main features short:
Fast curing with good repositioning time
Universally applicable for various types of applications and surfaces

PDP Technical Attributes Sum:
Chemical base: PU | Viscosity: 50,000 mPas | Hardening: 2 h | Tensile shear strength: Steel/Steel: ~ 5.4 N/mm², AL/AL: ~ 8.0 N/mm², ABS/PVC: ~ 3.7 N/mm², GRP/GRP: ~ 1.8 N/mm² | Temperature resistance: -40°C - +120°C

Application areas:
Plastic-plastic bonding as well as plastic repair and plastic-metal bonding, wood bonding
For all types of structural bonding in the automotive and truck sectors as well as in transport
Perfect solution for medium sized parts where workpieces may need to be repositioned. Such as bumpers, side mirrors, spoilers, interior parts bonding, roof racks, panels

Product advantages:
Fast curing with good repositioning time. 90 seconds tack free
Very vibration resistant. High adhesive strength with lasting flexibility
Long-lasting adhesion. Oil and grease resistant. Water and salt water resistant. Resistant to ageing
Very good processability. Can be sanded, drilled and painted over
Free from solvents and other VOCs

Hints:
Store in a cool, dry place and protect from sunlight
For the 25ml version use the mixing nozzle #207814 and for the 50ml version use the mixing nozzle #103480.
Please note that from August 24, 2023, appropriate training on the safe handling of diisocyanates must be completed before use. Further information about the training can be found at a "https://www.safeusediisocyanates.eu" target="_blank" www.safeusediisocyanates.eu /a

Processing instructions:
Clean the surface with the Berner Plast-O-Fix cleaner and prepare the surface with the Berner Primer Plast-O-Fix. Allow the primer to evaporate for at least 5-10 minutes. Thermoplastics (PVC, PC, PMMA, etc.) can be primed with isopropyl alcohol (IPA). Other types of solvents may damage the surface. Make sure both chambers of the cartridge are open and not clogged. Attach the Berner mixing nozzle to ensure a 1:1 mixing ratio. Before starting the actual application, discard the first 5 cm. A correct mixing ratio is now ensured and the product is ready for use. For some repairs, using a reinforcing film on the back of holes and cuts may be beneficial. Contour films can help with modeling and shaping the adhesive. These films must be removed after curing
Request a quote

Compare products

{"one"=>"Select 2 or 3 items to compare", "other"=>"{{ count }} of 3 items selected"}

Select first item to compare

Select second item to compare

Select third item to compare

Compare